Stream velocity (m/s) in the domain at an early crystallization stage for different melt thicknesses: (a) 10 mm, (b) 20 mm and (c) 40 mm.

 
 
  Part of: Gonik MA, Baltaretu F (2018) Problem of attaining constant impurity concentration over ingot height. Modern Electronic Materials 4(2): 41-51. https://doi.org/10.3897/j.moem.4.2.38536