Tetragonal-to-monoclinic phase transition rate for 4.0YSZ, 4.0GdSZ and 4.0SmSZ crystals in local areas near indentations. Inset: indentation images with Raman spectra recording points marked

 
 
  Part of: Chislov AS, Borik MA, Kulebyakin AV, Lomonova EE, Milovich FO, Myzina VA, Reu AA, Ryabochkina PA, Sidorova NV, Tabachkova NYu (2024) Comparison of the structure and physicochemical properties of ZrO2 based crystals partially stabilized with Y2O3, Gd2O3 and Sm2O3. Modern Electronic Materials 10(1): 3-10. https://doi.org/10.3897/j.moem.10.1.122043