Diffraction patterns of (a) extruded and (b) SPS Sn0.9Pb0.1Te specimens at temperatures: (1) 20 °С; (2) 200 °С; (3) 300 °С; (4) 500 °С

 
 
  Part of: Lavrentev MG, Voronov MV, Ivanov AA, Panchenko VP, Tabachkova NYu, Tapero MK, Yarkov IYu (2023) Mechanical properties of medium-temperature thermoelectric materials based on tin and lead tellurides. Modern Electronic Materials 9(4): 185-192. https://doi.org/10.3897/j.moem.9.4.116423